EN45 is a silicon mangenese spring steel, supplied in the as rolled contition. This steel is suitable for oil hardening and tempering.

TYPICAL ANALYSIS

C.

Si.

Mn.

S.

P.

0.55%

1.75%

0.75%

0.05%

0.05%

Forging: Forge at 1150C.Annealing: Slow furnace cool from 840/900C.

Hardening: Pre heat slowly to 650/700C and thoroughly soak. Continue heating to the final hardening temperature of 870/930C and allow the component to be heated through. Quench in oil.

Tempering: Temper immediately after quenching whilst tools are still hand warm. Re-heat to the tempering temperature, soak for one hour per  25 millimetre of total thickness, 2 hours minimum, then cool in air. For most applications tempering will be between 400/550C.